Very easily cut, bright red colour dulls to brown oxide.

Usage will assist final checks.

Copper

Lead alloys will show boiling lead under oxy flame. Higher zinc alloys fume. Colour variation assists with usage check.

Bronze

Brass

COLOUR

Red to yellow

Won't oxy cut

Aust. stainless steel

Oxy cuts

Aust. manganese steel

OXY CUT TEST

Sparks

Austenitic Manganese and Stainless Steel

Copper, brasses, bronzes, lead, lead-tin, zinc alloys Aluminium alloys Magnesium & alloys

White

Magnesium burns brightly

Hard

Oxy cuts

High carb.

stee.

Fractured surface marks paper, chips smoothly & brittle

Chips tough & rough

Malleable or SG iron

Dull grey

Nickel

Soft silvery

Low alloy high tensile

Ability to harden, common usage, will confirm spark test selection

Med. carb steel

SPARK TEST

Work hardened Aust. stainless or hard ferrite stainless

Won't cut

OXY CUT TEST

Work hardened Aust. Mang. steel

Grey cast iron

Mild steel

Aluminium drosses

OXY FLAME

Aluminium & alloys Magnesium & alloys

Lead, tin & zinc alloys Lead cuts with penknife, common usage.

Light

Heavy

RELATIVE WEIGHT

Monel

Cuts easily

HACKSAW-FILE TEST

SPARK TEST

No Spark

Very Slightly Magnetic

Non Magnetic

MAGNETIC TEST

METAL IDENTIFICATION

Cst irons, Chromium steels, High alloy tool and die steels, Nickel

Stainless (Ferritic)

Bright chrome

COLOUR CHECK Easily separated by colour, chip, usage & fracture.

Files hard White cast iron, Martensitic stainless steel, High alloy tool & die steels

Files soft Malleable & SG irons Grey cast iron Ferritic Stainless Nickel

FILE TEST

Won't oxy cut

Oxy cuts Low alloy & plain carbon steels

OXY CUT TEST

Strongly Magnetic