Page 278 of 561

COLD REPAIR COMPOUNDS

knowledge is not available. If the base material is so corroded that there is nothing to weld on, a new part can be “casted” with the repair compound. Where distortion of base material is unacceptable.

Welding causes expansion and contraction; resulting in distortion of the work piece.

Where there is restricted space. Polymer products can, if necessary, be injected through small diameter holes.

Where specific properties are required.

In many cases polymer compounds have better properties than weld overlays. Specifically, chemical resistance and wear resistant properties are improved. Large surfaces that are worn are also much faster overlaid with polymer compounds than with weld bead overlays.

Where you need non-metal repairs. Cold repair systems offer solutions for rubber gasket repairs or moulding, as well as solutions for repair or joining of plastics and composite materials.