Page 183 of 561

NIFE-334 N

Nickel Iron Electrode for Cast Iron

Imprint

Unitor NIFE-334 N / NiFe-C1 Classifications

SFA/AWS A5.15

EN-ISO 1071

E NiFe-CL-A Approvals

E NiFe-CL-A1

N.A.

Type of current

AC DC+/-

Welding positions

PA

Materials to be welded

PB

PC

For welding and repair

DIN 1692 GTS-35-10 GTS-45-06 GTS-55-4 GTW-35-04 GTW-40-05 GTW-45-07 GTW-S 38-12

DIN 1693 G GG-40 G GG-50 G GG-60

Ni

Fe

C

47.0 - 56.0

42.0 - 48.0

1.4 - 2.0

Tensile strength MPa

Yield strength

MPa

Elongation Hardness % HB

375

300

12 180

DIN 1691 G G 10 G G 15 G G 20 G G 25 G G 30 G G 35

PF

PG

PE, PD

3.01

All weld metal composition

Typical mech. properties of weld metal

Welding data

Diameter mm.

Current range, A

3.2 4.0

75–100

85–160

Arc time **/ Deposition rate** Electrodes per electrode, sec.

Kg/h kg weld metal**

Fume class

90 70

0.9 1.8

45 30

2

3

* SDS available on request. ** 90% of max. amperage

Packaging data

Diameter mm.

Length mm.

Electrodes per box

Net weight, kg per box

Product No.

per box

Boxes per carton

3.2 4.0

350 350

68 51

2.2 2.4

096-699512 096-699520

6

6

Re-drying temperature: 200 °C (392 °F) for two hours.