LHL-319 N

LMA

Electrode for Low Temperature Steel

Elect

rode

Identification:

Imprint

Unitor LHL-319 N / 8018-C1 Classifications

SFA/AWS A 5.5

EN-ISO 2560-A

E 8018-C1

E 46 6 2 Ni B 32 H5

Approvals

DNV

GL

LR

BV

5YH10 6Y46H5 5Y42H5 5Y 40M H5

Type of current

AC DC+

Welding positions

PA

Materials to be welded

Pipe material

Boiler & pressure vessel steel (for low temp. applic.)

PB

PC

API 5 LX NF A36-205 NF A36-207 BS 1501 DIN 17102 NF A36-203 DIN 17280 NF A36-208 NF A36-204

Fine grained steel

Low temperature steel

3.01

ABS 3Y400H5

High strength steel

PF

PE, PD

X52, X56, X60

A37FP, A42FP, A48FP, A52FP A510FP, A530FP, A550FP 224-Gr. 490 to LT 60, 282

StE315 to StE460

E355D, E390D, E430D, E445D 11MnNi53, 13MnNi63, 14NiMn6, 10Ni14 1.5Ni 285/355 (15N6), 2.5Ni 285/355 (10N9)

E420T, E460T

Can also be used for welding CorTen steel and Mayari R steels.

All weld metal composition

Typical mech. properties of weld metal

C

Mn

Si

P

S

Ni

0.02 - 0.10

0.65 - 1.15

0.15 - 0.55

max. 0.020

max. 0.020

2.15 - 2.65

Tensile strength MPa

Yield strength

MPa

Elongation Impact value % ISO-V (J)

610 520

26 At –60°C = 105

Welding data

Diameter mm.

Current range, A

2.5 3.2

70–110

105–150

Arc time **/ Deposition rate** Electrodes per electrode, sec.

Kg/h kg weld metal**

Fume class

55 63

0.9 1.4

70 42

2

3

* SDS available on request. ** 90% of max. amperage

Packaging data

Diameter mm.

Length mm.

Electrodes per box

Net weight, kg per box

Product No.

per box

Boxes per carton

2.5 3.2

350 350

78 48

1.8 1.8

095-683631 095-683649

6

6

Re-drying temperature: 350 °C (662 °F) for two hours.